My biggest issue with my part-time, weekend hobby work is flash rust. I clean up parts nicely and then sometimes get into a situation where a job is tacked up or partially welded and I have to stop for the week and by the next weekend flash rust presents, sometimes in corners where physical brushing is difficult. I live in a salty environment so that doesn't help.
So this thread is to ask if you guys have any particular products that you use or can recommend, where you could flap disc a part clean, then spray or wipe a product on, then in the short to medium term clean it off with acetone or alcohol or heat just before welding?
As an example, maybe things like:
Boeshield T-9?
Cooking spray?
WD-40/CRC/etc?
Candle wax?
Preferably something dirt cheap (Boeshield probably excluded) and that dries quickly to a tacky or dry film or residue (WD-40/CRC probably excluded) and easy to remove (paint e.g. cold galv or primer excluded).
So this thread is to ask if you guys have any particular products that you use or can recommend, where you could flap disc a part clean, then spray or wipe a product on, then in the short to medium term clean it off with acetone or alcohol or heat just before welding?
As an example, maybe things like:
Boeshield T-9?
Cooking spray?
WD-40/CRC/etc?
Candle wax?
Preferably something dirt cheap (Boeshield probably excluded) and that dries quickly to a tacky or dry film or residue (WD-40/CRC probably excluded) and easy to remove (paint e.g. cold galv or primer excluded).